Understanding Chemical Recycling

The term Chemical Recycling is easily misunderstood because it is one word that refers to several unique processes and technologies. Chemical Recycling is also a term that has not been unanimously accepted and can also be referred to as Advanced Recycling and Recovery or Transformational Technologies. It is key to understanding these technologies to grasp chemical recycling advancements.

It is important to note that chemical recycling is different from mechanical recycling. Mechanical recycling includes the physical sorting, cleaning, shredding, and often the re-processing of used plastic into pellets for incorporation into new products. Chemical recycling alters the form of the used plastics itself. The resulting product is dependent on the technology used to chemically recycle the plastics.

Categories of Chemical Recycling

Chemical recycling is commonly categorized as purification, depolymerization, or feedstock recycling. Each category showcases different methods for recycling chemicals found in plastics.

Purification – Used plastic is dissolved in a solvent, after which a series of purification steps occur to separate the polymer from additives and contaminants. The polymer of interest can then be selectively precipitated out. This results in a largely unaffected polymer that can be reformulated into plastics. Target feedstocks include poly(vinyl chloride) (PVC), polystyrene (PS), polyethylene (PE) and polypropylene (PP). Generally, plastic waste is collected as a mixture of polymers. The primary challenge with chemical recycling using this technique is the separation and recycling of waste components selectively.

Depolymerization – Is the reverse of polymerization and yields either single-monomer molecules or shorter polymer fragments known as oligomers. Monomers are identical to those used in the preparation of polymers and because of this, the plastics prepared from depolymerization are similar in quality to virgin monomers. Target feedstock is limited to condensation polymers such as polyesters (PET), polyamides (PA), and polyurethanes. It cannot be used for addition polymers, such as PP, PE, and PVC. Types of depolymerization include the following:

  • Methanolysis – a method using methanol as the solvent can be performed on PET currently by several industrial plants.
  • Glycolysis – a method using glycol as the solvent can be performed on PET by existing industrial plants. This method is also commonly used to process polyurethanes.
  • Hydrolysis – a method using water as the solvent, is mostly being used on a laboratory scale and at pilot-plants. There are several projects targeted for commercial development over the next few years. Depolymerization of polyamides and polyurethanes are mainly carried out by this technique.
  • Ammonolysis/Aminolysis – methods using ammonia or amines as the solvent are considered less established and developed options.

Feedstock Recycling – Any thermal process that converts polymers into simpler molecules, in order to form the feedstock for petrochemical-type processing. The outputs of feedstock recycling are basic chemicals (e.g., hydrocarbons or synthetic gas), which need to be processed further to yield a polymer. This allows flexibility for reuse in the petrochemical industry. Chemical recycling thus relies on diverse methods to achieve recycling goals.

petroleum refinery

Petroleum refining plant.

Types of Feedstock Recycling

Feedstock recycling can be characterized further as pyrolysis, gasification, or hydrothermal treatment. Each method adds another layer to the chemical recycling toolkit available for tackling plastic waste.

Pyrolysis – Breaks plastics down into a range of basic hydrocarbons by heating in the absence of oxygen. Distillation is then used to change the hydrocarbon vapor into products ranging from heavy wax and oils to light oils and gas. Pyrolysis products can be processed in much the same way as oil, using conventional refining technologies to produce building blocks for polymers. Alternatively, they can be used directly as a fuel. Target feedstocks include PE, PP, polybutylene (PB), polystyrene (PS), and poly(methylmethacrylate) (PMMA). Pyrolysis of mixed plastics has been in development over the last two decades, but it is only now becoming a reality with several commercial plants in operation with many more expected to be commissioned over the next few years.

Gasification – A process where mixed waste materials are pretreated to remove moisture and then heated to a very high temperature in the presence of a limited amount of oxygen, which breaks the molecules down to their simplest components. Gasification of waste plastics leads to the production of syngas, made up of mainly hydrogen (H2), carbon monoxide (CO), carbon dioxide (CO2), methane (CH4) and nitrogen (N2). This gas can be burnt for energy or used in the production of new hydrocarbons along with a variety of chemicals. Target feedstocks include all plastics. Gasification of mixed waste has been in use for quite some time. Gasification plants are typically built at a larger scale than pyrolysis plants.

Hydrothermal Treatment – The essential reactions of HTT are hydrolysis, dehydration, decarboxylation, and depolymerization. Hydrothermal treatment has been proposed as a solution for the separation of mixed waste (MW) into organic and inorganic substances. The main product is synthetic crude oil – separation, purification, and upgrading can then be handled by standard refinery operations. Target feedstocks include plastic packaging waste (PET), carbon fiber reinforced plastics (CFRP), printed circuit boards (PCB), polycarbonate, styrene-butadiene, poly(lactic acid), nylon 6, and nylon 66. Technology is at a development stage, with commercial operations in planning. Chemical recycling through hydrothermal means aims to leverage various processes for efficient recycling.

Outlook for Chemical Recycling
North America will play an important role in the future of chemical recycling. Resin manufacturers, like BASF and Eastman Chemical Co., will continue to take the lead on the commercialization of chemical recycling technologies. Innovation in chemical recycling techniques promises a more sustainable future.

Status of chemical recycling

Figure 1. Forecast of chemical recycling by region for 2030.

Even though the outlook on chemical recycling is strong, it will not negate mechanical recycling. Therefore it is important that we continue to make positive progress in the area of mechanical recycling while balancing the benefits of both mechanical and chemical recycling in our efforts.

forecast of global plastics production through 2050

Figure 2. Forecast of global plastics production through 2050.

Melissa L. Kurtz, M.S.

Melissa Kurtz is a Managing Engineer at The Madison Group. Melissa holds an M.S. degree in Material Science and Engineering from Wayne State University. She has over 20 years of experience serving the global product development community across several industries including transportation, medical, and consumer products. She is an expert in material selection, test method development, and failure analysis.