Creep Failure of Plastics – WEBINAR

September 21, 2023 @ 10:00 am - 11:00 am CDT

Register for this webinar event here:
Creep Failure of Plastics

Creep is the tendency of a polymeric material to deform permanently under the influence of constant stress, as applied through tensile, compressive, shear, or flexural loading. It occurs as a function of time through extended exposure to levels of stress that are below the yield strength of the material. Given sufficient time, this can lead to creep rupture, the failure within a material as a result of continuously applied stress at a level below the tensile strength. Plastic materials are particularly prone to creep rupture through exposure to static stresses, and a recent study indicates that 22% of plastic failures are associated with creep.

The relatively high frequency of creep failure is linked to the widespread lack of awareness and understanding of the effects of time on polymeric materials, particularly at the design stage; the unique difference in time dependence between polymeric materials and metals; and the increasing use of plastic materials in diverse applications with longer time demands.

The concept of creep is extremely important to manufacturers and users of plastic components.

This webinar will cover:

  • Introduction to Creep
  • Plastics Failure Mechanism
  • Creep Failure Mechanism
  • Generalizations of Creep
  • Creep Testing and Lifetime Projection
  • Creep Failure Case Studies