The Problem

Toolmaker Carlson Tool and Manufacturing had to determine if their proposed cooling line layout was optimized and would achieve turbulent flow for maximizing cooling efficiency in a twelve-cavity injection mold. The Madison Group used injection molding simulation for cooling optimization of the cooling layout design and quantify how much coolant was required to achieve turbulent flow and reduced cycle times.

Download Case Study PDF

The Madison Group

The Madison Group is the recognized leader in plastics engineering. Over three decades, The Madison Group has focused on polymeric materials. We understand how these materials behave, how to properly design with them, how they are processed, and the numerous manufacturing steps required to produce a successful product.